Sign In | Join Free | My himfr.com
Home > Nickel Alloy Plate >

GH4180 alloy:nickel-based superalloy with high strength, excellent oxidation resistance, and high-temperature stability

Jiangsu Zhonggongte Metallurgical Technology Co., Ltd.
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now
    Buy cheap GH4180 alloy:nickel-based superalloy with high strength, excellent oxidation resistance, and high-temperature stability from wholesalers
     
    Buy cheap GH4180 alloy:nickel-based superalloy with high strength, excellent oxidation resistance, and high-temperature stability from wholesalers
    • Buy cheap GH4180 alloy:nickel-based superalloy with high strength, excellent oxidation resistance, and high-temperature stability from wholesalers
    • Buy cheap GH4180 alloy:nickel-based superalloy with high strength, excellent oxidation resistance, and high-temperature stability from wholesalers

    GH4180 alloy:nickel-based superalloy with high strength, excellent oxidation resistance, and high-temperature stability

    Ask Lasest Price
    Brand Name : Zhonggong Special Metallurgy
    Model Number : GH4180 alloy
    Price : Price is negotiated based on the required specifications and quantity
    Payment Terms : Payment Terms: Mainly T/T.. L/C, D/A, D/P,
    Supply Ability : 5000 tons per month
    Delivery Time : 5-8 working days, depending on the parameters required for negotiation
    Certification : ISO Certificate
    • Product Details
    • Company Profile

    GH4180 alloy:nickel-based superalloy with high strength, excellent oxidation resistance, and high-temperature stability

    GH4180 Alloy

    GH4180 is a high-performance nickel-based superalloy designed for superior strength and oxidation resistance in extreme environments. It is specifically engineered for applications requiring high-temperature stability and durability.

    Key Features:

    • Composition: Primarily composed of nickel, with significant amounts of chromium, iron, cobalt, and molybdenum, enhancing its mechanical properties and resistance to thermal degradation.
    • Temperature Resistance: GH4180 performs reliably at high temperatures up to approximately 1390°C (2530°F), maintaining its structural integrity and mechanical properties under severe thermal conditions.
    • Mechanical Strength: The alloy offers high yield and tensile strength, making it suitable for high-stress applications where robust performance is critical.
    • Oxidation and Corrosion Resistance: GH4180 excels in resisting oxidation and high-temperature corrosion, ensuring longevity and reliability in aggressive environments.
    • Applications: Commonly used in aerospace components, gas turbines, and high-temperature industrial processes, GH4180 is ideal for environments where high strength and excellent resistance to thermal and environmental stresses are essential.

    GH4180’s unique combination of high strength, thermal stability, and corrosion resistance makes it an excellent choice for demanding applications in aerospace and industrial sectors.


    This description highlights GH4180 alloy's key attributes and typical applications, providing a comprehensive overview of its performance and benefits.


    Here’s a detailed composition table for GH4180 alloy:

    ElementContent Range
    Nickel (Ni)Balance
    Chromium (Cr)19.0-21.0%
    Iron (Fe)9.0-11.0%
    Cobalt (Co)8.0-10.0%
    Molybdenum (Mo)2.0-3.0%
    Titanium (Ti)2.0-3.0%
    Aluminum (Al)1.0-2.0%
    Boron (B)0.005-0.015%

    This table provides a clear overview of GH4180 alloy's chemical composition, detailing the content ranges of its key elements.


    Quality GH4180 alloy:nickel-based superalloy with high strength, excellent oxidation resistance, and high-temperature stability for sale
    Inquiry Cart 0
    Send your message to this supplier
     
    *From:
    *To: Jiangsu Zhonggongte Metallurgical Technology Co., Ltd.
    *Subject:
    *Message:
    Characters Remaining: (0/3000)